Zn Anodes
| |  |
|
For the manufacturing of zinc anodes we use high-purity
(99.99 %) Zn blocks.
The melting procedure takes place in the induction
furnace, in graphite melting pots, with the application
of the metallurgically necessary covering and cleansing
salts. The alloy will be cast in oxide-, and inclusionfree
state. The surfaces of the connections are coated by
a zinc layer. The form casting of the blocks is carried
out by means of cast iron moulds according to the US
MILL, BS, DIN standards.
| Composition: | Standard
Al: max. 0,5
Fe: max. 0,05
Cn: max. 0,05
Cd: max. 0,05
Pb: max. 0,005
Zn: the rest | US MILL
Al: 0,10-0,50
Fe: max. 0,005
Cn: max. 0,005
Cd: 0,025-0,07
Pb: max. 0,006
Zn: the rest |
 |
| A | B | C | D | Insert | Net
(kg) | Gross
(kg) |
| I | 500 | 230 | 47 | 55 | 12 | 10 | 11 |
| II | 1000 | 230 | 47 | 55 | 12 | 20 | 22.5 |
| III | 1250 | 230 | 55 | 60 | 12 | 29.5 | 31 |
| IV | 1250 | 230 | 55 | 65 | 12 | 32 | 33.6 |
| V | 1250 | 230 | 63 | 80 | 12 | 45 | 46.5 |
| VI | 1500 | 230 | 70 | 80 | 12 | 60 | 61.5 |
|
 |
| A | B | C | D | Diameter | Net
(kg) | Gross
(kg) |
| H1 | 200 | 120 | 40 | 25 | 10X3 | 0.5 | 0.55 |
| H2 | 260 | 180 | 60 | 32 | 20X3 | 1 | 1.1 |
| H3 | 300 | 220 | 75 | 38 | 20X3 | 2.15 | 2.3 |
| H4 | 380 | 290 | 100 | 50 | 30X5 | 4.65 | 5 |
| H5 | 400 | 280 | 150 | 75 | 40X6 | 10 | 10.7 |
| H6 | 520 | 420 | 160 | 70 | 40X6 | 15 | 16 |
|
|  |